facebook_icon
Metals > Copper > 1093 > Ex Spring

Copper 1093 Ex Spring

MECHANICAL PROPERTY LIMITS
Tensile Strength Yield Strength Elongation Rockwell B Hardness*
x1000PSI(N/mm²=KSI x 6.895)
x1000PSI(Kgf/mm²=KSI x .7031)
nominal % in 2in.
(=% in 50 mm.)
Nominal .020" gauge and over
52 min 51 min 3 max
  • Yield Strength - x1000PSI(Nominal .2% offset)(N/mm²=KSI x 6.895)
  • Yield Strength - x1000PSI(Nominal .2% offset or range)(Kgf/mm²=KSI x .7031)
  • Rockwell F, 30T, 15N, or H where noted
CHEMICAL COMPOSITION LIMITS (%)
ASTM Spec Number Nominal Composition Density Module of Elasticity Electric Conductivity Thermal Conductivity Coefficient of Thermal Expansion
(a) (b) (c) (d) (e)
B152 Cu-Min. 99.9
Ag Min. 13 oz./ton
0.322 17 101 226 9.8
  • (a) X 106 PSI, tension (Kgf/mm² = KSI x .7031)
  • (b) % IACS AT 68°F (20°C) as annealed
  • (c) BTU•ft. @ 68°F ft²•hr•F (20°C)
  • (d) Inches/inch/°F x 10-5 from 68°F to 572°F (20°C to 300°C)
Slitting Capabilities
Gauge Range
.004" to .187" (.102 mm to 4.750 mm)
Width Range
.250" to 60" (6.365 mm to 1524 mm)
ID
8, 12, 16 or 20 (inches)
OD
78" maximum
Coil Weight
40,000 lbs maximum
Cut-to-Length Capabilities
Gauge Range
.012 to .045 (.305 mm to 1.143 mm)
Width Range
8” - 48” (203 mm to 1.219 mm)
Length Range